On the thermo-mechanical behaviour of DEMO water-cooled lithium lead equatorial outboard blanket module
2017
Abstract Within the framework of EUROfusion R&D activities an intense research campaign has been carried out at the University of Palermo, in close cooperation with ENEA Brasimone, in order to investigate the thermo-mechanical performances of the DEMO water-cooled lithium lead breeding blanket (WCLL). In particular, attention has been paid to the most recent geometric configuration of the DEMO WCLL outboard equatorial module, as designed by WCLL project team during 2015, endowed with an attachment system based on the use of radial pins, purposely outlined to connect the module back-plate to its back-supporting structure, that have been properly considered to simulate more realistically the …
A constitutive model for the thermo-mechanical behaviour of fusion-relevant pebble beds and its application to the simulation of HELICA mock-up exper…
2007
Abstract Within the framework of the R&D activities promoted by EFDA on the Helium-Cooled Pebble Bed Test Blanket Module to be irradiated in ITER, attention has been focused on the modelling of the thermo-mechanical behaviour of both beryllium and lithiated ceramic pebble beds that are envisaged to be used respectively as neutron multiplier and tritium breeder. This behaviour depends, mainly, on the reactor-relevant conditions, the pebble sizes and the breeder cell geometries and a general constitutive model has not yet been validated, especially for fusion-relevant applications. ENEA-Brasimone and the Department of Nuclear Engineering (DIN) of the University of Palermo have performed inten…
Progress in the benchmark exercise for analyzing the lithiate breeder pebble bed thermo-mechanical behaviour
2006
The Helium Cooled Pebble Bed (HCPB) Blanket is one of the reference concepts for the European Breeding Blanket Programme for DEMO. In the reference blanket module, alternate layers of lithiated ceramics and beryllium pebbles act, respectively, as tritium breeder and neutron multiplier. The thermo-mechanical behaviour of both the pebble beds and their performances in reactor relevant conditions are also dependent on the pebble size and cell geometries (bed thickness, pebble packing factor, bed thermal conductivity). Therefore, in the EU Fusion Technology Programme, several out-of-pile experimental test campaigns have been performed to determine these behaviours. Theoretical calculations have…
Analysis of the thermo-mechanical behaviour of the DEMO Water-Cooled Lithium Lead breeding blanket module under normal operation steady state conditi…
2015
Within the framework of DEMO R&D activities, a research cooperation has been launched between ENEA, the University of Palermo and CEA to investigate the thermo-mechanical behaviour of the outboard equatorial module of the DEMO1 Water-Cooled Lithium Lead (WCLL) blanket under normal operation steady state scenario. The research campaign has been carried out following a theoretical-computational approach based on the Finite Element Method (FEM) and adopting a qualified commercial FEM code. In particular, two different 3D FEM models (Model 1 and Model 2), reproducing respectively the central and the lateral poloidal-radial slices of the WCLL blanket module, have been set up. A particular attent…
Thermo-mechanical testing of Li-ceramic for the helium cooled pebble bed (HCPB) breeding blanket
2004
The helium cooled pebble bed (HCPB) Test blanket module (TBM) for the DEMO Reactor foresees the utilization of lithiate ceramics as breeder in form of pebble beds. The pebbles are organized in several layers alternatively stacked among couples of cooling plates (CP). ENEA has launched an experimental programme for the out-of-pile thermo-mechanical testing of mock-ups simulating a portion of the HCPB-TBM. The programme foresees the fabrication and testing of different mock-ups, to be tested in the HE-FUS3 facility at ENEA Brasimone. The paper describes the HELICHETTA III campaign carried-out in 2003. In particular, the test section layout, the pebble filling procedure, the experimental set-u…
On thermo-mechanical issues induced by irradiation swelling inside the back-plate of the IFMIF target assembly
2011
Abstract Within the framework of the IFMIF R&D program and in close cooperation with ENEA-Brasimone, at the Department of Nuclear Engineering of the University of Palermo a research campaign has been launched to investigate the thermo-mechanical issues potentially induced by irradiation swelling in the threaded connections between frame and back-plate of IFMIF target assembly. The main aim of the research campaign has relied in the assessment of the maximum swelling-induced volumetric strain that may be accepted in order to allow screws to withstand thermo-mechanical stresses and work in safe conditions or to avoid unduly high unscrewing torques during back-plate remotely handled maintenanc…
Electro Thermo Mechanical Characterization of NiTi Actuator Wire
2010
Assessing the MALDI-TOF MS sample preparation procedure to analyze the influence of thermo-oxidative ageing and thermo-mechanical degradation on poly…
2011
[EN] Multiple processing by means of successive injection cycles was used to simulate the thermo-mechanical degradation effects on the oligomeric distribution of PLA under mechanical recycling. Likewise, an accelerated thermal ageing over PLA glass transition was performed in order to simulate its service life. MALDI-TOF MS was used for the analysis and the sample preparation procedure was assessed by means of a statistical Design of Experiments (DoE). The quality effects in use for the analysis were signal-to-noise ratio and Resolution. Different matrixes, analyte/matrix proportions and the use of NaTFA as cationization agent were considered. A deep inspection of the statistical results pr…
1994
Polymer blends can undergo, during processing, degradation phenomena because of the presence of both temperature and mechanical stresses. With respect to pure homogeneous polymers, the degradation of polymer blends shows distinct features because of the possible interaction between the different chemical species. These interaction can give rise to both a faster degradation or to the formation of copolymers which act as stabilizing agents. This latter phenomena is particularly important in the processing of condensation polymers